Bubbles and voids
Pin holes, voids and unstable bubbles can appear when moisture reaches the die. Check the resin, storage and drying record before changing the grade.
DM2476G is a desiccant masterbatch for film and bags, used where drying alone does not hold the line on PE or recycled film.
Share the resin, film structure, moisture history, current dosage and defect. The team reviews carrier, CaO level, colour effect and trial conditions by exact grade before a sample or quote.
Water turns to steam under melt temperature. Thin film shows the result before a thick part does, and recycled or humid resin makes the window narrower.
Pin holes, voids and unstable bubbles can appear when moisture reaches the die. Check the resin, storage and drying record before changing the grade.
Moisture-related splay and surface disturbance can raise haze. Confirm the film thickness and lighting before comparing samples.
Recycled film can carry moisture and variation from storage, washing and regrind. The desiccant route is reviewed with the stream, not as a universal fix.
Feeder accuracy, screw speed and output change the delivered dose. The trial has to record the line, not only the masterbatch percentage.
The current TDS positions DM2476G as a CaO desiccant masterbatch in a recycled PE carrier. These values belong to that grade and revision, not to every desiccant masterbatch.
| Property | TDS example | Film check |
|---|---|---|
| DM2476G | 75.9% CaO | Moisture load, dosage and film thickness |
| Carrier | 24% recycled PE | Buyer recycled-content rules and resin compatibility |
| CaCO3 filler | 0% | Film specification and surface requirement |
| Starting addition | 1% | Actual moisture, feeder calibration and trial result |
| TDS applications | Film blowing, injection, extrusion | Line, film structure and final use |
* Current TDS example. Packaging: 5 kg vacuum bags, five per 25 kg carton. Addition range is a starting point, not a fixed dosage. Confirm the current grade, revision, carrier and packaging for the offered product.
The desiccant is one variable in a moisture problem. These checks keep the trial tied to the film and the line.
Record where the defect appears, the film thickness and the line conditions. A bubble is a symptom, not proof of the material source.
Check for undispersed particles and gels. The carrier and dispersion route matter as much as the CaO content.
The recycled PE carrier and CaO can affect film appearance. Define the acceptable colour and haze before the trial.
Confirm that the buyer specification accepts the 24% recycled PE carrier before the grade is standardised.
Start from the current TDS 1% point and verify the feeder output. Do not treat the starting point as a fixed answer for every film.
Use the same resin, film structure, thickness and machine as the control. Keep the batch and actual dose with the samples.
Four steps, with the moisture source and film result reviewed before a commercial offer.
Resin, recycled stream, storage, drying, film structure and defect.
Carrier, CaO level, starting dose, colour effect and document scope.
Agree the control, dose and line conditions before judging the film.
TDS, COA, SDS and compliance scope are reviewed by exact grade and application.
It is a CaO-based concentrate added to the resin to bind free moisture during processing. The aim is to reduce moisture-related bubbles, voids and surface defects, not to replace every resin drying step.
The current TDS lists a 1% starting point. Treat it as a starting point and confirm the actual dose on the line, because moisture load, film thickness, output and feeder accuracy change the result.
No. It can support moisture control, but the resin, storage and drying process still have to be reviewed. A desiccant masterbatch is not a substitute for identifying why the moisture is there.
DM2476G is a grey CaO masterbatch in a recycled PE carrier. The colour and haze effect has to be checked against the film target, especially in thin or natural-colour film.
It can be reviewed for recycled PE film, but the stream, contamination, moisture history and buyer recycled-content rules have to be confirmed. The grade still needs a trial on the actual line.
Food-contact suitability is not a product-line claim. It depends on the exact grade, application, market and the corresponding documents. Those points are reviewed separately.
Send the resin, recycled stream, film structure, moisture history and current defect. The team will review DM2476G and the trial conditions before a quote or sample.